Why are there rough marks or stains left on the brass handle?
After seeing information that welding marks, dents, or discoloration may be visible on the handle, one wants to confirm whether it is a product defect or a manufacturing characteristic.
It is made using a traditional handcrafted method where the aluminum body and brass handle are joined by hand, leaving natural traces from the processing and welding procedures.
The body is shaped from aluminum, and the handle is fitted separately with heavy brass[1]. It is made by hand. Ottinetti produces kitchenware that can be used for a long time by combining aluminum and brass using traditional handcrafted methods[2].
In general, brass easily develops fine scratches or uneven surfaces during the process of being welded and hammered into shape at high temperatures. As an alloy of copper and zinc, it also reacts with air or moisture, causing partial oxidation into darker colors. Because of this, welding marks, scratches, dents or contours, as well as coloring caused by metal reactions, are revealed as they are on the handle's surface[3][4].



The official cleaning method for managing discoloration and stains that form on the surface of the brass handle has not yet been confirmed.
Product measurements
View details
[오티네티] 투티 프루티 과일 스탠드
Other stated figures
| Part | Value |
|---|---|
| 무게 | 565g |
[오티네티] 미니 편수냄비 높은형 (2size / 뚜껑O)
Other stated figures
| Part | Value |
|---|---|
| 두께 | 2.8mm |
| 도자기 ◦ | 3cm |
For rows marked with ◦, flat measurement or circumference could not be confirmed in official sources, so hmmm determined them using figures from the same item.
[오티네티] 후라이팬 (3size)
Other stated figures
| Part | Value |
|---|---|
| 두께 | 1.2mm |
![[오티네티] 투티 프루티 과일 스탠드](https://img.hmmm.pub/brands/ottinetti/products/21b141ae-b4d2-4cc5-8f16-560b4f16caa7/2.jpg)